If you’ve ever worked with heat exchangers, chemical processing equipment, or high-pressure fluid transfer systems, you’ve likely encountered spirally wound stainless steel tubes. As a supplier who’s been manufacturing these for nearly 15 years, I’ve seen firsthand how a seemingly simple design can hide subtle defects that cause big headaches for project teams, from delayed timelines to costly system failures. A lot of new engineers and even veteran plant managers underestimate how the winding process—where flat stainless steel strips are wrapped tightly around a mandrel, sealed with welds, and formed into a continuous tube—creates unique vulnerabilities that aren’t present in seamless or extruded tubes. Today, I want to break down the most common defects I run into, what causes them, and how we work to prevent them at our facility, because knowing these issues upfront can save you thousands in downtime and replacement parts. Spirally Wound Stainless Steel Tube

The first, and arguably most critical, defect is interlayer delamination. This happens when the bond between two adjacent layers of the spirally wound strip fails, leaving a gap that lets fluid seep between layers instead of flowing through the tube’s intended inner path. At its core, this defect traces back to improper weld penetration or surface contamination during the winding process. Early in my career, we had a batch of tubes rejected by a chemical plant because they leaked after only three months of service—testing revealed that the interlayer welds had only penetrated 60% of the strip thickness, not the required 100% for 316L stainless steel. What had happened was that a technician swapped out a fresh roll of strip for one that had been sitting in our warehouse in a corrugated cardboard box, and residual adhesive from the box hadn’t been fully wiped off before loading. That adhesive created a barrier so the weld head couldn’t fuse the layers properly. Now, every incoming strip gets a two-step cleaning: first with industrial alcohol to remove any surface debris, then a visual inspection by a second operator before it goes to the winding line. We also use ultrasonic testing (UT) on every batch post-production to catch low weld penetration before tubes leave our dock.
Closely related to delamination is void formation in the weld seams between the spirally wound edges. These tiny, gas-filled gaps in the longitudinal weld that joins the start and end of each strip layer might seem small, but they act as stress concentrators. Over time, especially in systems cycling between high pressure and room temperature, those voids can expand into cracks. I remember a food processing client that installed our tubes in a pasteurization line; within a year, one section ruptured during a pressure test. When we investigated, we found that the welds had trapped hydrogen gas during the welding process, a common issue if the shielding gas flow was too low. Our team adjusted our argon shielding parameters to maintain a 20 L/min flow rate during welding, and we added a post-weld heat treatment (PWHT) for all tubes used in cyclic pressure applications to diffuse any trapped hydrogen. We also use X-ray radiography on 10% of every batch’s welds as a secondary check, which cuts down on these void-related defects by over 90% compared to our early days.
Another underdiscussed defect is ovality, or the deviation of the tube’s cross-section from a perfect circle. Spirally wound tubes are formed by winding strip around a mandrel, but if the winding tension is uneven or the cooling process after welding is inconsistent, the tube can end up flattened, especially on the side where the strip is joined. For applications like heat exchangers, where the tube has to fit tightly into a tube sheet, even 1 mm of ovality can cause gaps that lead to poor thermal transfer or, worse, the tube moving and damaging the surrounding components. I once worked with a construction firm that ordered 50 tubes for a coastal desalination project; they rejected half because we had missed the ovality check. The issue was that our mandrel had a small warp, so as the tube was wound, the tension pulled more on one side. We replaced the mandrel and installed laser alignment tools to measure cross-section diameter at three points along each tube, and now every shipment comes with a digital ovality report for this exact reason. For critical applications, we also offer mandrel-mounted sizing after winding to correct any minor deformations before the final weld is applied.
Surface pitting is a defect that doesn’t show up right away, but it’s deadly in corrosive environments, like those with saltwater or acidic chemicals. Pitting occurs when chloride ions or other corrosive agents get trapped on the tube’s surface, usually in small scratches left by the winding process or residual mill scale that wasn’t removed. A mining client once had a tube fail in a leaching system after six months, and the root cause was a 0.5 mm scratch from the winding machine’s guide rollers that had trapped acidic solution. The pit grew inward until it perforated the tube wall. To fight this, we use a passivation process on all finished tubes: after cutting and deburring, we submerge the tubes in a nitric acid solution to remove any free iron from the surface, which prevents the formation of these pitting sites. We also inspect every tube under a 10x magnifier before shipment to catch any scratches or surface defects that could lead to pitting later on.
One defect that’s often hard to spot until the tube is in service is longitudinal cracking, not from welds, but from the base material itself. Wait—spirally wound tubes use flat stainless steel strips, right? Well, if the strip has internal laminations from the rolling process before it reaches us, those laminations can open up during winding, especially if the tension is too high. I’ve seen a few cases where a supplier’s raw strip had hidden laminations, and when we wound it at standard tension, a crack ran along the length of one layer. That’s why we now perform edge crushing tests on every coil of strip we receive: we bend a small section of the strip around a mandrel of equal diameter to our finished tubes, and if cracks form at the edges, we reject the entire coil. It’s an extra step that adds a bit of time, but it’s saved us from dozens of bad tubes going out.
Thickness variation is another common defect that impacts performance, even if it’s not a visible issue. Spirally wound tubes are designed with a consistent wall thickness to handle pressure, but if the winding speed fluctuates, or the strip feed mechanism slips, the wall can be thinner in some areas. For high-pressure applications, like oil and gas flow lines, a 0.2 mm difference in wall thickness can reduce the tube’s pressure rating by up to 20%, which is a huge safety risk. To prevent this, we use servo-controlled feed rollers that maintain a constant strip tension within ±5% during winding, and we use ultrasonic thickness gauging to scan every tube at 100 points along its length. That way, we catch any thin spots before the tube is shipped.
Of course, none of these defects are unavoidable. At our facility, we’ve built our quality control process around understanding each of these issues, because when a customer’s equipment fails, it’s not just our reputation on the line—it’s their production, their safety, and their bottom line. If you’re working on a project that uses spirally wound stainless steel tubes, don’t wait for a defect to cause problems. We can help you test your existing tubes for any of these issues, or supply custom-made tubes tailored to your specific application, with full quality documentation that covers all the checks we’ve discussed today.

If you’re looking to replace defective tubes, or you’re designing a new system and want to avoid these common pitfalls, get in touch with us to discuss your requirements. We work with projects of all sizes, from small industrial workshops to large-scale chemical plants, and we’ll make sure your tubes are manufactured to meet your exact standards, no exceptions.
Threaded Stainless Steel Tube References
- ASME Boiler and Pressure Vessel Code, Section VIII, Division 1: Rules for Construction of Pressure Vessels, American Society of Mechanical Engineers, 2023.
- “Defects in Welded Tubes and Their Mitigation,” International Journal of Pressure Vessels and Piping, Vol. 189, 2021, pp. 104267.
- Stainless Steel Tube Manufacturing Process Handbook, Nickel Institute, 2020.
- Ultrasonic Testing for Welded Tubular Products, American Society for Nondestructive Testing, 2019.
- “Corrosion Resistance of Spirally W Austenitic Stainless Steel Tubes,” Corrosion Science, Vol. 165, 2020, pp. 108452.
China Super Tech Co., Ltd.
As one of the most professional spirally wound stainless steel tube manufacturers and suppliers in China, we’re featured by quality products and good service. Please rest assured to wholesale OEM spirally wound stainless steel tube from our factory. Also, custom service is available.
Address: Wangjing Science and Technology Park, Guangshun North Street, Chaoyang District, Beijing
E-mail: sales@316liquidcooling.com